Creep Testing Machine

Creep Testing Machine Manufacturers & OEM Suppliers from India

Engineering Lab Equipment Material Testing Equipment

Creep Testing Machine

Product Code LTEKCTLB-MT03-1013

Description & Specification

Creep Testing Machine

Technical Specifications

A sturdy bench top mounted unit for studying the affect of creep on different material test specimens. Necked test specimens are held vertically in position on special clamps, which do not induce bending during loading. A lever arm transmits the load from a load hanger and weights into the specimen and the lever arm has a counter balance weight to ensure the lever arm self weight is calibrated out.

Surrounding the test specimen is a transparent specimen guard. Its primary function is to allow the surrounding specimen temperature to be adjusted hot or cold. The temperature can be read using the thermometer supplied and the temperature controlled using a special thermal pack. The specimen cover also allows easy viewing of the specimen during creep. A dial gauge measures the extension of the specimen during testing. Specimens in polypropylene are supplied as standard. Specimens in nylon and PVC are also available as optional sets.

Data generated using creep & creep-rupture test allows for predicting creep modulus as well as strength of materials that are under constant loads is also used for predicting dimensional changes occurring as result of such loads
Data generated from test methods finds usage in –
Comparing materials
In designing fabricated parts
For characterizing plastics for achieving long-term performance under constant loads

FEATURES:
Creep fracture load
Temperature affect on creep rate and failure
Material variation on creep rate and failure
Load variation on creep rate and failure

SPECIFICATIONS:
To be bench mounted unit to study creep within different material
Uniform, stable load to be applied using lever arm
Creep test specimens to be held in position by clams which do not induce bending
Test temperature to be controlled within transparent specimen cover
Thermometer supplied
Ability for the test specimens to be heated and cooled
Load hanger and weights set for applying load to creep specimen
Dial gauge measures displacement during creep
10 specimens in Polypropylene to be supplied
Spare test specimens to be available
Why choose LTekOnline

Trusted Creep Testing Machine Manufacturer & Supplier

LTekOnline are the manufacturers of Creep Testing Machine used to demonstrate engineering principles in Engineering Colleges, Engineering Schools, and Material Testing Equipment for Engineering Teaching Lab in Universities. We supply Creep Testing Machine to TVET institutes, vocational training centres, polytechnics and research labs across more than 90 countries, with quality testing technology, comprehensive operation manuals and full after-sales support.

  • Manufactured to international standards
  • Detailed operation & experiment manuals
  • Turnkey lab installation & training
  • Worldwide shipping & on-site support
20000+ Lab Products
90+ Countries Served
2000+ Turnkey Projects

Need a Quote for Creep Testing Machine?

Get a custom quote, technical datasheet, or schedule a virtual demo with our lab equipment specialists. We respond within 24 hours.